G
4

Question about forge welding. I was struggling with a 3/8 inch mild steel bar for a gate hinge. Kept getting cold shuts. Tried flux paste instead of powder for once, and it actually stuck on the first heat.

2 comments

Log in to join the discussion

Log In
2 Comments
mary_schmidt
Flux paste is way less messy than the powder.
2
dakotal19
dakotal192d ago
Which brand of paste do you find works best for SMD rework?
3