Tried pre-heating a 3/4 inch rolled shell before rolling it and got a surprise I wasn't ready for
So about three weeks back I had a small shell job in the shop, 3/4 inch plate, maybe 40 inches around, nothing crazy. I'd read somewhere that warming a rolled shell a bit before you finish rolling helps it hold the curve better and cuts down on springback, so I figured what the heck, I'll give it a shot with the rosebud. I got it to maybe 400 degrees, nice and even, and went back to the rolls. Well, the shell came out of the rolls looking great, I'm feeling pretty smart, and then I set it down and it kept moving on me. Sat there creaking and popping for a good ten minutes while it cooled, and by the time it settled the gap at the seam had opened up almost a half inch from where I had it. I had to chase it back with the rolls and re-fit the whole thing, which took me an extra hour and a half. Lesson is the heat does help it roll easier, but you better plan for it shrinking while it cools or you're fitting a moving target. Any of you heat your shells before rolling, or is that just me making extra work for myself?
Wait, it moved a half inch on you? That's wild for a 3/4 plate. I've never preheated a shell before rolling and now I'm glad I haven't, because I would've done the exact same thing, pat myself on the back and then watch it walk on me while it cools. Ten minutes of creaking and popping would've had me thinking the thing was coming apart. Did the plate cool down even, or did you get any warping from the rosebud? Seems like chasing that seam back with the rolls is the only way out once it shrinks like that.